Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Monprene® RG-10130 - TPE - Teknor Apex Co.

Material Data Center offers the following functions for Monprene® RG-10130:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Monprene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Preliminary Data

The Monprene RG-10100 series is a group of high performance thermoplastic elastomers specifically designed for regulated applications including food contact, toys, and children's products. Monprene RG-10130 is a low density, low hardness grade that complies with various US FDA and European regulations and directives for food contact and toy safety and is suitable for injection molding.

Adheres to PP

PropertyValueUnitStandard
Tensile Stress at 100% (across flow)0.48MPaISO 37
Tensile Stress at Break (across flow)4.2MPaISO 37
Tensile Strain at Break (across flow)860%ISO 37
Tear Strength (across flow)6.2kN/mISO 34-1
Apparent Viscosity (200 °C, 206 1/s)204PasASTM D3835
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 1.5 g/10min ASTM D 1238
温度 200 °C -
荷重 5 kg -
機械的特性単位テスト基準
ISO データ
圧縮永久ひずみ 70℃, 24h 20 % ISO 815
引裂強さ 12 kN/m ISO 34-1
ショア硬さA 29 - ISO 7619-1
その他の特性.単位テスト基準
密度 888 kg/m³ ASTM D 792
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 65 °C -
Pre-drying - Time 2 - 4 h -
樹脂温度 182 - 227 °C -
金型温度 27 - 49 °C -
Zone 1 160 - 177 °C -
Zone 2 182 - 204 °C -
Zone 3 182 - 216 °C -
Nozzle temperature 182 - 227 °C -
Screw speed 50 - 100 rpm -
Back pressure 0.172 - 0.689 MPa -
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
添加剤.
滑剤.
特殊な特性.
Translucent
な特性
Good Adhesion
Certifications
Food contact, Food approval FDA 21 CFR
アプリケーション
パッケージング
領域別の利用可能性
北アメリカ., ヨーロッパ., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com