Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Maxxam" in Material Data Center leads to the following information:

Tradename: Maxxam
Family: PE-HD, PE-LD, PE-LLD, PP
Producer: Avient Corporation
130 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Maxxam™ 34-1520 SSM TFPP PP-T20
Maxxam™ 34-1520 UV SSM TFPP PP-T
Maxxam™ 8400-7001 PP-K30
Maxxam™ BL-818.G001-1017 PP-GF40
Maxxam™ BL-818.H001-8016 PP-GF40
Maxxam™ CL2 GF/30 BLACK PP-GF30
Maxxam™ DC-818.G001-8000 PP-(GX+MX)30
Maxxam™ DP 9052-3-1000 (PE-HD)-GF15
Maxxam™ DP-9156-5-8000 PP-GF10
Maxxam™ DP-9162-3 PP
Maxxam™ ET5200-8016 RS Natural PP-GF40
Maxxam™ F5134T2-4 PP-(T+MX)21
Maxxam™ F5134T4-1 PP-(T+MX)40
Maxxam™ FR C5 T-GF/10 XF V0 EP NC 70 PP-(GF+MX)10
Maxxam™ FR H6 GF/30 XF V0 NC 70 PP-GF30
Maxxam™ FR H6 T/05 H XF V0 NATURAL 70 PP-MX
Maxxam™ FR MF5210-0301 DK GRAY 2451 PP
Maxxam™ FR MF5420-0013 FR (PE-LD)
Maxxam™ FR MF5420-0085 NHFR PP
Maxxam™ FR PE 112 Natural RoHS (PE-LD)
Maxxam™ FR PE 161-1A Natural (PE-HD)
Maxxam™ FR PE CONC 1 NAT (PE-LD)
Maxxam™ FR PE126 BLK 3330 (PE-LD)
Maxxam™ FR PO Conc 62 (PE-LD)
Maxxam™ FR PP 301 BLK 1284-11 S PP
Maxxam™ FR PP 301 EXT PP
Maxxam™ FR PP 301 NATL S PP
Maxxam™ FR PP 301 NATL S-30 PP
Maxxam™ FR PP 307 PP
Maxxam™ FR PP 401 PP
Maxxam™ FR PP 402 PP
Maxxam™ FR PP 600 PP
Maxxam™ FR PP CONC 36 NAT S PP
Maxxam™ FR PP Concentrate 4 PP
Maxxam™ FR PP FR 7A11 PP
Maxxam™ FR PP FR 7B01 PP
Maxxam™ FR PP FR 7B11 BK287 PP
Maxxam™ FR PP FR 7B31 PP
Maxxam™ FR PP FR 7C11 PP
Maxxam™ FR PP H6 GF25 NHFR grey PP
Maxxam™ FR PP301 SHI BK268 PP
Maxxam™ FR PP301 SHI NC196 PP
Maxxam™ FR PP301S WT ROHS PP
Maxxam™ FR WC 0521-48 R1 RoHS PP
Maxxam™ FR WC 0587-21 R2 RoHS PP
Maxxam™ FW-818.G001-8706 PP-GF10
Maxxam™ GV-819.G001-1001 PP-GF30
Maxxam™ GV-819.G001-8065 PP-GF30
Maxxam™ MAXBATCH YM-618.G001-1000 PP-T70
Maxxam™ MD 4245-1000 PP-K30
Maxxam™ MD 4245-59770 PP-K30
Maxxam™ MN-818.S001-8000 PP-GF40
Maxxam™ MN-818.T001-8001 PP
Maxxam™ MX5200-5004 RS BLACK PP-(T+MX)
Maxxam™ MX5200-5005 RS BLACK PP-(T+MX)
Maxxam™ MX5200-5006 RS NATURAL PP-(T+MX)
Maxxam™ MX5210-0040 RS Natural PP-GF40
Maxxam™ NM-718.G002-1704 PP-GF25
Maxxam™ NM-719.S001-8042 PP-GF20
Maxxam™ NM-818.H001-1049 PP-GF20
Maxxam™ NM-818.H001-8046 PP-GF
Maxxam™ NR-218.S001-8080 PP-MX
Maxxam™ NR-818.G001-1062 PP-MX
Maxxam™ NR-818.H001-8086 PP-MX
Maxxam™ NS-818.G001-1032 PP-MX
Maxxam™ NT-818.B001-8000 PP-GF16
Maxxam™ NT-818.G002-8000 PP-X25
Maxxam™ NX-818.E041-8002 PP-CF10
Maxxam™ PD 2201 PP-T20
Maxxam™ PD 40 TF Black PP-T40
Maxxam™ PE GF/10 Natural 70 NA (PE-HD)-GF
Maxxam™ PP 301 BLK 1284-11 S PP
Maxxam™ PP 301(f2) NC713 PP
Maxxam™ PP 5120C PP-(T+MX)21
Maxxam™ PP 6120 B38 BK PP-MX
Maxxam™ PP FR 7380-8001 PP
Maxxam™ PP FR 7B01 BK439 PP
Maxxam™ PP301 BLK PP
Maxxam™ PP301 NC PP
Maxxam™ PP5120 A1 PP-(T+MX)21
Maxxam™ PP5120 B4 PP-(T+MX)21
Maxxam™ PP5120R B2 PP-T
Maxxam™ PP5120R B2 SO1 PP-(K+GX)
Maxxam™ PP5140F D30 PP-(T+MX)40
Maxxam™ PP5226 E132 PP-(K+GX)
Maxxam™ PP5930 Black PP-GF30
Maxxam™ PP5930R B1 PP-GF30
Maxxam™ PP6 BK021 PP-MX
Maxxam™ PPC-10G Black PP-GF
Maxxam™ PPC-10G Nat PP-GF10
Maxxam™ PPC-20C Nat PP-K20
Maxxam™ PPC-20G Black PP-GF20
Maxxam™ PPC-20G Nat PP-GF20
Maxxam™ PPC-20T Black PP-T20
Maxxam™ PPC-20T Nat PP-T20
Maxxam™ PPC-30T UV EXT 1148 PP-T30
Maxxam™ PPC-40C Nat PP-K40
Maxxam™ PPC-40G Black PP-GF40
Maxxam™ PPC-40T Nat PP-T40
Maxxam™ PPH-10G Nat PP-GF10
Maxxam™ PPH-20C Nat PP-K20
Maxxam™ PPH-20G Black PP-GF20
Maxxam™ PPH-20G Nat PP-GF20
Maxxam™ PPH-30T Nat PP-T30
Maxxam™ PPH-40C Nat PP-K40
Maxxam™ PPH-40G Black PP-GF40
Maxxam™ PPH-40G Nat PP-GF40
Maxxam™ PPH-40T Nat PP-T40
Maxxam™ PPR 40G BK701 PP-GF
Maxxam™ PPR-20G Black PP-GF20
Maxxam™ PPR-20G Nat PP-GF20
Maxxam™ PPR-30G Nat PP-GF30
Maxxam™ PPR-40G Black PP-GF40
Maxxam™ PPR-40G Nat PP-GF40
Maxxam™ RB 135601 TPO
Maxxam™ SY 89-21-1 PP
Maxxam™ SY 89-22-7 PP
Maxxam™ SY 89-23-7 PP
Maxxam™ TH-418.G001-1390 PP
Maxxam™ TH-418.S001 6770 PP
Maxxam™ TR-818.G001-8081 PP-T30
Maxxam™ VS-418.H001-1702 PP-GF
Maxxam™ VS-693.G001-8009 PP-GF
Maxxam™ VS-818.G001-1023 PP-GF10
Maxxam™ XN-418.G001-1000 PP-K40
Maxxam™ FR PP FR 8-6 A NATURAL - ROHS PP-T
Maxxam™ FR QD 813.Y001-1000 RoHS PP-GF30
Maxxam™ FR QD 818.Y001 PP-GF30
Maxxam™ FR WC 0587-21 BE1 RoHS PP
Maxxam™ PD 20 TF Black PP-T23

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.