Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® LED5902 FR RE - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® LED5902 FR RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 6 cm³/10min ISO 1133
温度 300 °C -
荷重 1.2 kg -
成形収縮率, 平行 0.7 % ISO 294-4, 2577
成形収縮率, 直角 0.7 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 2300 MPa ISO 527
降伏応力 66 MPa ISO 527
降伏ひずみ 6.2 % ISO 527
破壊呼びひずみ >50 % ISO 527
破壊応力 60 MPa ISO 527
破壊ひずみ 60 % ISO 527
曲げ弾性率, 23°C 2400 MPa ISO 178
曲げ強さ 99 MPa ISO 178
シャルピー衝撃強さ, +23°C N kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C, 3mm 32 kJ/m² ISO 179/1eA
ノッチ付きIzod衝撃強さ, +23°C 50[1] kJ/m² ISO 180/1A
パンクチャー衝撃-最大応力, +23゚C 5100 N ISO 6603-2
パンクチャー衝撃-最大応力, -30゚C 6100 N ISO 6603-2
パンクチャー衝撃エネルギー, +23゚C 50 J ISO 6603-2
パンクチャー衝撃エネルギー, -30゚C 55 J ISO 6603-2
Ball indentation hardness 120 MPa ISO 2039-1
1: 3 mm
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 121 °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 136 °C ISO 75-1/-2
ビカット軟化温度, B 142 °C ISO 306
厚さhでの燃焼性 V-0 class IEC 60695-11-10
試験片の厚さ 1.0 mm -
厚さhでの燃焼性 5V 5VA class IEC 60695-11-20
試験片の厚さ 3.0 mm -
酸素指数 39 % ISO 4589-1/-2
グローワイヤ燃焼性指数 (GWFI) 960 °C IEC 60695-2-12
GWFI - 試験片の厚さ 0.75 mm -
グローワイヤ燃焼性指数 (GWFI) 960 °C IEC 60695-2-12
GWFI - 試験片の厚さ 1.5 mm -
グローワイヤ燃焼性指数 (GWFI) 960 °C IEC 60695-2-12
GWFI - 試験片の厚さ 3 mm -
グローワイヤ着火温度 (GWIT) 850 °C IEC 60695-2-13
GWIT - 試験片の厚さ 0.75 mm -
グローワイヤ着火温度 (GWIT) 850 °C IEC 60695-2-13
GWIT - 試験片の厚さ 1.5 mm -
グローワイヤ着火温度 (GWIT) 850 °C IEC 60695-2-13
GWIT - 試験片の厚さ 3 mm -
光学特性単位テスト基準
ISO Data
ヘイズ 1 - ISO 14782
視感透過率 89 % ISO 13468-1, -2
Other Standards[S]
くっせつりつ 1.58 - ISO 489
S: These properties are reported by the producer according standards that are different to our defaults.
その他の特性.単位テスト基準
密度. 1200 kg/m³ ISO 1183
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 120 °C -
Pre-drying - Time 4 h -
樹脂温度 280 - 320 °C -
金型温度 80 °C -
特殊な特性
成形加工法.
射出成形.
添加剤.
離型剤.
特殊な特性.
難燃., 紫外線安定化., 透明.
Certifications
Contains renewable resources, ISCC Plus
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.