Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Amphora™ 3D Polymer HT5300 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Amphora™ 3D Polymer HT5300:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Amphora datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Application/Uses
-Production of 3D Printing Filaments

Eastman Amphora™ HT5300 3D polymer is a low-odor, and styrene-free material uniquely

suited for advanced 3D printing users, particularly those who need their creations to exhibit

superior durability, dimensional stability, toughness, and high temperature resistance.The

model of functional aesthetics, Amphora HT5300 can be made into high-quality filament that

exhibits advanced overhang ability, excellent toughness and temperature resistance, good

looks, and superior melt strength—empowering professional users to create durable, more

useful items. Demonstrating superior dimensional stability, BPA-free HT5300 allows for 3D

printing to exacting dimensions, which is especially important for products with tight tolerances

and multi-component parts. Moreover, with its outstanding toughness and chemical

resistance, Amphora HT5300 is ideal for prototyping and testing products, especially for

applications that require temperature resistance up to 100°C.

機械的特性単位テスト基準
ASTM数据
降伏応力 43 MPa ASTM D 638
破壊応力 52 MPa ASTM D 638
降伏点伸び 7 % ASTM D 638
破断伸び 210 % ASTM D 638
曲げ弾性率 1575 MPa ASTM D 790
曲げ強さ 64 MPa ASTM D 790
ロックウェル硬度 R 111 - ASTM D 785
ノッチ付きIzod衝撃強さ, 1/8 in 860 J/m ASTM D 256
アイゾット衝撃試験, 1/8 in N J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
DTUL @ 66 psi 94 °C ASTM D 648
DTUL @ 264 psi 81 °C ASTM D 648
その他の特性.単位テスト基準
密度 1180 kg/m³ ASTM D 792
特殊な特性
成形加工法.
Additive Manufacturing
特殊な特性.
熱安定化.
な特性
High Gloss, Low Odor, Melt Strength, Copolymer
耐薬品性
General Chemical Resistance
Certifications
Food contact, Food approval FDA 21 CFR
アプリケーション
電気電子, Filament for 3D Printing
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com