Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Akromid C" in Material Data Center leads to the following information:

Tradename: Akromid C
Family: PA66+PA6
Producer: Akro-Plastic GmbH
34 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
AKROMID® C3 1 FR black (5266) (PA66+PA6)
AKROMID® C3 GF 25 1 FR black (7246) (PA66+PA6)-GF25
AKROMID® C3 GF 25 1 FR natural (7208) (PA66+PA6)-GF25
AKROMID® C3 GF 30 1 FR black (7243) (PA66+PA6)-GF30
AKROMID® C3 GF 30 1 FR natural (7207) PA666-GF30
AKROMID® C3 GF 30 5 XTC black (4686) (PA66+PA6)-GF30
AKROMID® C28 GF 25 FRT natural (7332) PA*
AKROMID® C3 1 FR black (4361) PA666
AKROMID® C3 1 FR grey (4298) (PA66+PA6)
AKROMID® C3 5 S3 black (21013) (PA66+PA6)
AKROMID® C3 GF 35 5 XTC black (5552) (PA66+PA6)-GF35
AKROMID® C3 GF 35 5 XTC black (6680) (PA66+PA6)-GF35
AKROMID® C3 GF 50 5 XTC natural (4946) (PA66+PA6)-GF50
AKROMID® C3 GF 30 5 XTC natural (4499) (PA66+PA6)-GF30
AKROMID® C3 GF 35 1 black (4668) (PA66+PA6)-GF35
AKROMID® C3 GFM 15/25 1 black (6653) (PA66+PA6)-(MX+GF)40
AKROMID® C3 GF 30 1 black (4363) (PA66+PA6)-GF30
AKROMID® C3 1 S3 black (4297) (PA66+PA6)
AKROMID® C3 GF 35 1 natural (4748) (PA66+PA6)-GF35
AKROMID® C3 ICF 30 5 XTC black (5473) (PA66+PA6)-CF30
AKROMID® C28 GFM 10/20 5 XTC black (7367) (PA66+PA6)-(MD+GF)30
AKROMID® C3 1 black (4546) (PA66+PA6)
AKROMID® C3 5 S3 black (4605) (PA66+PA6)
AKROMID® C3 GF 15 5 XTC natural (5088) (PA66+PA6)-GF15
AKROMID® C3 GF 30 1 FR orange (7855) (PA6+PA66)-GF30
AKROMID® C3 GF 40 1 black (4658) (PA66+PA6)-GF40
AKROMID® C3 GF 50 1 black (4401) (PA66+PA6)-GF50
AKROMID® C3 GF 60 1 black (4659) (PA66+PA6)-GF60
AKROMID® C28 GF 25 FRT blue (7986) PA*-GF25
AKROMID® C28 GF 25 FRT grey (7560) PA*-GF25
AKROMID® C28 M 30 6 black (7934) PA66/6-MX30
AKROMID® C3 1 FR natural (8050) (PA66+PA6)
AKROMID® C3 3 S3 ECO black (8163) (PA66+PA6)
AKROMID® C3 GF 25 1 FR orange (7854) PA66/6-GF25

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.