Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Akroloy - PA66+PA6I/6T - Akro-Plastic GmbH

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Akroloy" in Material Data Center leads to the following information:

Tradename: Akroloy
Family: PA66+PA6I/6T
Producer: Akro-Plastic GmbH
56 hits in the material database
4 hits in the literature database
1 hits in the application database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
AKROLOY® PARA GF 50 1 black (7583) PARA-GF50
AKROLOY® PA GF 50 black (6507) (PA66+PA6I/6T)-GF50
AKROLOY® PA GF 50 natural (6414) (PA66+PA6I/6T)-GF50
AKROLOY® PARA GF 50 1 natural (5750) PARA-GF50
AKROLOY® PARA ICF 40 black (6128) PARA-CF40
AKROLOY® PA GF 40 black (6416) (PA66+PA6I/6T)-GF40
AKROLOY® PA GF 50 black (6546) (PA66+PA6I/6T)-GF50
AKROLOY® PA GF 50 natural (7573) (PA66+PA6I/6T)-GF50
AKROLOY® PA GF 60 natural (6465) (PA66+PA6I/6T)-GF60
AKROLOY® PA ICF 30 black (5269) (PA66+PA6I/6T)-CF30
AKROLOY® PARA GF 35 FR black (7496) PARA-GF35
AKROLOY® PARA GF 50 1 natural (5913) PARA-GF50
AKROLOY® PARA GF 60 1 natural (6165) PARA-GF60
AKROLOY® PA GF 30 natural (6412) (PA66+PA6I/6T)-GF30
AKROLOY® PA GF 50 8 black (6732) (PA66+PA6I/6T)-GF50
AKROLOY® PA GF 60 black (6765) (PA66+PA6I/6T)-GF60
AKROLOY® PA ICF 20 black (5268) (PA66+PA6I/6T)-CF20
AKROLOY® PA ICF 40 black (5270) (PA66+PA6I/6T)-CF40
AKROLOY® PA LGF 50 natural (5504) (PA66+PA6I/6T)-GF50
AKROLOY® PA GF 50 black (2706) (PA66+PA6I/6T)-GF50
AKROLOY® PA GF 60 7 black (2844) (PA66+PA6I/6T)-GF60
AKROLOY® PA GF 30 black (2718) (PA66+PA6I/6T)-GF30
AKROLOY® PA GF 30 8 black (6730) (PA66+PA6I/6T)-GF30
AKROLOY® PA GF 50 natural (2916) (PA66+PA6I/6T)-GF50
AKROLOY® PA GF 60 black (6418) (PA66+PA6I/6T)-GF60
AKROLOY® PA GF 60 7 natural (2941) (PA66+PA6I/6T)-GF60
AKROLOY® PA GF 60 8 black (6733) (PA66+PA6I/6T)-GF50
AKROLOY® PA K17 FR black (5762) PA66-GF35...
AKROLOY® PA GF 30 natural (3177) (PA66+PA6I/6T)-GF30
AKROLOY® PA GF 40 black (2845) (PA66+PA6I/6T)-GF40
AKROLOY® PA GF 50 grey (3807) (PA66+PA6I/6T)-GF50
AKROLOY® PA CF 40 black (3639) (PA66+PA6I/6T)-CF40
AKROLOY® PA GF 30 black (6415) (PA66+PA6I/6T)-GF30
AKROLOY® PA GF 30 8 black (4171) (PA66+PA6I/6T)-GF30
AKROLOY® PA GF 40 natural (3059) (PA66+PA6I/6T)-GF40
AKROLOY® PA GF 40 natural (6413) (PA66+PA6I/6T)-GF40
AKROLOY® PA GF 50 natural (5930) (PA66+PA6I/6T)-GF50
AKROLOY® PA GF 50 8 natural (6606) (PA66+PA6I/6T)-GF50
AKROLOY® PA ICF 10 black (5267) (PA66+PA6I/6T)-CF10
AKROLOY® PA M 40 natural (2972) (PA66+PA6I/6T)-MX40
AKROLOY® PARA LGF 50 1 natural (5824) PARA-GF50
AKROLOY® PA GF 40 HU black (8149) (PA66+PA6I/6T)-GF40
AKROLOY® PA GF 40 HU natural (8148) (PA66+PA6I/6T)-GF40
AKROLOY® PA GF 50 HU black (8198) (PA66+PA6I/6T)-GF50
AKROLOY® PA GF 50 white (5137) (PA66+PA6I/6T)-GF50
AKROLOY® PA GF 60 beige (7632) (PA66+PA6I/6T)-GF60
AKROLOY® PA GF 60 black (8054) (PA66+PA6I/6T)-GF60
AKROLOY® PA GF 60 HU black (8153) (PA66+PA6I/6T)-GF60
AKROLOY® PA GF 60 HU natural (8152) (PA66+PA6I/6T)-GF60
AKROLOY® PA GF 60 LA black (8168) (PA66+PA6I/6T)-GF60
AKROLOY® PA M 40 black (6541) (PA66+PA6I/6T)-MX40
AKROLOY® PARA GF 30 black (7841) PARA-GF30
AKROLOY® PARA GF 35 FR grey (8200) PARA-GF35
AKROLOY® PARA GF 35 FR natural (8038) PARA-GF35
AKROLOY® PARA GF 50 8 black (8026) PARA-GF50
AKROLOY® PARA ICF 40 black (6129) PARA-CF40

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.