Caratteristiche Fisiche | Valore | Unitá | Norma del test |
Other Standards[S] |
Indice di fluidità a caldo, MFI |
8 |
g/10min |
ASTM D 3307 |
Temperatura |
372 |
°C |
- |
Carico |
5 |
kg |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Meccaniche | Valore | Unitá | Norma del test |
Other Standards[S] |
Resistenza alla trazione |
28 |
MPa |
ASTM D 3307 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Termiche | Valore | Unitá | Norma del test |
Other Standards[S] |
Temperatura di fusione |
285 |
°C |
ASTM D 4591 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Elettriche | Valore | Unitá | Norma del test |
Other Standards[S] |
Resistività volumica |
0.11 |
Ohm*m |
ISO 3915 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Altre Proprietà | Valore | Unitá | Norma del test |
Densità |
2150 |
kg/m³ |
ASTM D 792 |
Caratteristiche
Processabilità e Forma di Forni
Altre Estrusioni, Soffiaggio, Stampaggio a Trasferimento, Stampaggio a compressione
Forma fisica disponibile
Pellet
Caratteristiche speciali
Antistatico, Estab. agli U.V. o per applicaz.in esterni
Caratteristiche
Resistenza al scorrimento, Resistenza del fuso, Stabilità termica, Grado tribologico
Resistenza Chimica
Resistenza chimica generale, Resistenza ai solventi
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.