Caratteristiche Fisiche | Valore | Unitá | Norma del test |
Other Standards[S] |
Indice di Fluiditá, MFI |
12 |
g/10min |
DIN 53735 |
Temperatura |
220 |
°C |
- |
Carico |
10 |
kg |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Meccaniche | Valore | Unitá | Norma del test |
ISO Data |
Resist. urto Charpy con intaglio, +23°C |
12 |
kJ/m² |
ISO 179/1eA |
Resistenza all'urto Izod con intaglio, +23°C |
22 |
kJ/m² |
ISO 180/1A |
Other Standards[S] |
Modulo a trazione |
2300 |
MPa |
DIN 53457 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Termiche | Valore | Unitá | Norma del test |
Other Standards[S] |
Temp.di rammollimento Vicat, B |
92 |
°C |
DIN 53460 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Altre Proprietà | Valore | Unitá | Norma del test |
Other Standards[S] |
Massa volumica |
1060 |
kg/m³ |
DIN 53479 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Caratteristiche
Forma fisica disponibile
Nero
Caratteristiche speciali
Alto urto o modificato all'urto
Disponibilità geografica
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com