Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ DN003 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ DN003:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

Eastar™ Copolyester DN003 contains a mold release. It has excellent appearance and is nearly water-clear. This polymer is the toughest of the Eastar™ family of products. Additional outstanding features are chemical resistance and excellent color and property retention following gamma and e-beam sterilization.




Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Ritiro di stampaggio, parallelo 0.0035 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Carico unitario a trazione 46 MPa ISO 527
Deformazione a snervamento 4.4 % ISO 527
Carico unitario a rottura 47 MPa ISO 527
Deformazione a rottura 230 % ISO 527
Modulo a flessione, 23°C 1800 MPa ISO 178
Resistenza all'urto Izod con intaglio, +23°C 125 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio 7.4 kJ/m² ISO 180/1A
Temperatura -40 °C -
Energia di perforazione, +23°C 14 J ISO 6603-2
ASTM Data
Resistenza alla trazione di snervamento 45 MPa ASTM D 638
Resistenza alla trazione a rottura 52 MPa ASTM D 638
Allungamento a snervamento 5 % ASTM D 638
Allungamento a rottura 330 % ASTM D 638
Modulo a flessione 1800 MPa ASTM D 790
Durezza Rockwell 105 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in N J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 64 J/m ASTM D 256
Temperatura -40 °C -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 65 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 74 °C ISO 75-1/-2
Temp.di rammollimento Vicat, A 88 °C ISO 306
Temp.di rammollimento Vicat, B 79 °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.6 mm -
Reazione al fuoco a spessore h HB class IEC 60695-11-10
Spessore provato 3.2 mm -
ASTM Data
UL 94 combustibilitá HB - UL 94
Spessore testati 1.6 mm -
DTUL a 66 psi 74 °C ASTM D 648
DTUL a 264 psi 64 °C ASTM D 648
Temp.di rammollimento Vicat 88 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1230 kg/m³ ISO 1183
Assorbimento d’acqua, 24hr 0.13 % ASTM D 570
Densità 1230 kg/m³ ASTM D 792
Raccomandazione de Processabilità EstrusioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 71 °C -
Pre-essiccamento - Tempo 6 h -
Temperatura di fusione 250 - 270 °C -
Temperatura dello stampo 15 - 40 °C -
Caratteristiche
Processabilità e Forma di Forni
Altre Estrusioni
Forma fisica disponibile
Colore naturale
Additivi
Agente di distacco
Caratteristiche speciali
Alto urto o modificato all'urto, Trasparente, Sterilizzabile, Gamma irradiation sterilization, Electron beam (e-beam) sterilization
Caratteristiche
Proprietà di barriera, High Gloss, Copolimero
Resistenza Chimica
Resistenza chimica generale, Resistenza ai solventi, Resistenza alla radiazione
Applicazioni
Medicale
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.