Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PLA - PLA - BASF

Material Data Center offers the following functions for Ultrafuse PLA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 21.2 cm³/10min ISO 1133
Temperature 220 °C -
Load 5 kg -
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 151 °C ISO 11357-1/-3
Glass transition temperature, 10°C/min 61 °C ISO 11357-1/-2
Temp. of deflection under load, 1.80 MPa 55 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 65 °C ISO 75-1/-2
Other propertiesValueUnitTest Standard
Density 1250 kg/m³ ISO 1183
3D DataValueUnitTest Standard
Other Standards[S]
Tensile modulus, flat 2310 MPa ISO 527
Tensile modulus, upright 2130 MPa ISO 527
Tensile strength, flat 34.7 MPa ISO 527
Tensile strength, upright 21.2 MPa ISO 527
Strain at break, flat 4.2 % ISO 527
Strain at break, upright 1.2 % ISO 527
Flexural modulus, flat 1860 MPa ISO 178
Flexural modulus, on-edge 1710 MPa ISO 178
Flexural modulus, upright 1720 MPa ISO 178
Flexural strength, flat 98 MPa ISO 178
Flexural strength, on-edge 105 MPa ISO 178
Flexural strength, upright 54.9 MPa ISO 178
Charpy impact strength, +23°C, flat 13.2 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, on-edge 14.3 kJ/m² ISO 179/1eU
Charpy impact strength, +23°C, upright 4.3 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C, flat 2.5 kJ/m² ISO 179/1eA
Charpy notched impact strength, +23°C, on-edge 1.9 kJ/m² ISO 179/1eA
Charpy notched impact strength, +23°C, upright 1.7 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, flat 11 kJ/m² ISO 180/1U
Izod impact strength, +23°C, on-edge 9.6 kJ/m² ISO 180/1U
Izod impact strength, +23°C, upright 4.7 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C, flat 3.3 kJ/m² ISO 180/1A
Izod notched impact strength, +23°C, on-edge 2.1 kJ/m² ISO 180/1A
Izod notched impact strength, +23°C, upright 1.6 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Characteristics
Processing
Additive Manufacturing
Delivery form
Monofilament
Features
Low Warpage
Certifications
Contains renewable resources
Regional Availability
North America, Europe, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com