Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ WX500 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ WX500:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastman Tritan™ WX500 copolyester is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generation copolyester

most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. Tritan WX500 copolyester may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations.

Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.006 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1570 MPa ISO 527
Yield stress 45 MPa ISO 527
Yield strain 7 % ISO 527
Stress at break 51 MPa ISO 527
Strain at break 142 % ISO 527
Flexural modulus, 23°C 1490 MPa ISO 178
Flexural strength 60 MPa ISO 178
Izod notched impact strength, +23°C 78 kJ/m² ISO 180/1A
Izod notched impact strength 12 kJ/m² ISO 180/1A
Temperature -40 °C -
ASTM Data
Tensile Modulus 1609 MPa ASTM D 638
Tensile Strength at Yield 45 MPa ASTM D 638
Tensile Strength at Break 52 MPa ASTM D 638
Elongation at Yield 7 % ASTM D 638
Elongation at Break 139 % ASTM D 638
Flexural Modulus 1522 MPa ASTM D 790
Rockwell Hardness R 110 - ASTM D 785
Izod Impact notched, 1/8 in 842 J/m ASTM D 256
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 101 °C ASTM D 648
DTUL @ 264 psi 85 °C ASTM D 648
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 1 % ASTM D 1003
Light Transmittance 91 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1180 kg/m³ ASTM D 792
Characteristics
Processing
Blow Molding
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat, Transparent
Features
Melt Strength, Copolymer
Chemical Resistance
General Chemical Resistance, Hydrolytically Stable
Certifications
Food contact, Food approval FDA 21 CFR
Applications
Packaging
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.