Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ TX1000 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ TX1000:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts

Eastman Tritan TX1000 is an amorphous copolyester with excellent appearance and clarity. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. This new-generation copolyester can also be molded into various applications without incorporating high levels of residual stress.

Combined with Eastman Tritan™ copolyester’s outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity and aggressive cleaning detergents. Tritan TX1000 copolyester may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations. Tritan TX1000 is certified to NSF/ANSI Standard 51 for Food Equipment Materials.




Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Mold Shrinkage, MD 0.006 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 1550 MPa ISO 527
Yield stress 47 MPa ISO 527
Yield strain 7 % ISO 527
Stress at break 58 MPa ISO 527
Strain at break 185 % ISO 527
Flexural modulus, 23°C 1500 MPa ISO 178
Flexural strength 59 MPa ISO 178
Izod notched impact strength, +23°C 93 kJ/m² ISO 180/1A
Izod notched impact strength 20 kJ/m² ISO 180/1A
Temperature -40 °C -
ASTM Data
Tensile Modulus 1550 MPa ASTM D 638
Tensile Strength at Yield 43 MPa ASTM D 638
Tensile Strength at Break 53 MPa ASTM D 638
Elongation at Yield 6 % ASTM D 638
Elongation at Break 210 % ASTM D 638
Flexural Modulus 1550 MPa ASTM D 790
Rockwell Hardness R 112 - ASTM D 785
Izod Impact notched, 1/8 in 980 J/m ASTM D 256
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 99 °C ASTM D 648
DTUL @ 264 psi 85 °C ASTM D 648
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 1 % ASTM D 1003
Light Transmittance 90 % ASTM D 1003
Other propertiesValueUnitTest Standard
Density 1180 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 88 °C -
Pre-drying - Time 4 - 6 h -
Melt temperature 260 - 282 °C -
Mold temperature 38 - 66 °C -
Characteristics
Processing
Injection Molding, Profile Extrusion
Special Characteristics
High impact or impact modified, Heat stabilized or stable to heat, Transparent
Features
Amorphous, Copolymer
Chemical Resistance
General Chemical Resistance, Hydrolytically Stable
Certifications
Food contact, Food approval FDA 21 CFR, Food approval NSF 51
Applications
Building Construction, Electrical and Electronical, Packaging, Sports Equipment
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.