Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TOYOLAC® 920 - ABS - Toray Industries, Inc.

Material Data Center offers the following functions for TOYOLAC® 920:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Toyolac datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index 25 g/10min ASTM D 1238
Temperature 220 °C -
Load 10 kg -
Mold Shrinkage, MD 0.004 mm/mm ASTM D 955
Mold Shrinkage, TD 0.006 mm/mm ASTM D 955
Density 1090 kg/m³ ASTM D 792
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength 48 MPa ASTM D 638
Elongation at Break 20 % ASTM D 638
Flexural Modulus 2160 MPa ASTM D 790
Flexural Strength 74 MPa ASTM D 790
Rockwell Hardness R 115 - ASTM D 785
Izod Impact notched, 1/8 in 0.104 kJ/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
UL 94 Flame rating HB - UL 94
DTUL @ 264 psi 83 °C ASTM D 648
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 4 % ASTM D 1003
Light Transmittance 87 % ASTM D 1003
Characteristics
Processing
Injection Molding, Other Extrusion
Special Characteristics
Transparent
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright M-Base Engineering+Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from M-Base; this is especially valid for claims of compensation resulting from consequential damages. M-Base explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: 2017-01-20 Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.