Toyolac - ABS, SAN - Toray Industries, Inc

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Toyolac" in Material Data Center leads to the following information:

Tradename: Toyolac
Family: ABS, SAN
Producer: Toray Industries, Inc
80 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
TOYOLAC® 100 322 ABS
TOYOLAC® 100 MPF ABS
TOYOLAC® 100-MPM ABS
TOYOLAC® 100 X01 ABS
TOYOLAC® 100G-10 ABS-GF10
TOYOLAC® 100G-20 ABS-GF20
TOYOLAC® 100G-30 ABS-GF30
TOYOLAC® 250-X10 ABS
TOYOLAC® 250-SG5 ABS
TOYOLAC® 325 ABS
TOYOLAC® 440Y MH1 ABS
TOYOLAC® 440Y MH5 ABS
TOYOLAC® 450Y MH1 ABS
TOYOLAC® 450Y MH5 ABS
TOYOLAC® 450Y-X10 ABS
TOYOLAC® 470Y MH1 ABS
TOYOLAC® 470Y-X68 ABS
TOYOLAC® 500 322 ABS
TOYOLAC® 532-X02 ABS
TOYOLAC® 560-X17 ABS
TOYOLAC® 600-309 ABS
TOYOLAC® 700-314 ABS
TOYOLAC® 700-X01 ABS
TOYOLAC® 700-SG5 ABS
TOYOLAC® 824V-X01 ABS
TOYOLAC® 834V-X01 ABS
TOYOLAC® 834V-X06 ABS
TOYOLAC® 844V-X05 ABS
TOYOLAC® 855VG20 ABS-GF20
TOYOLAC® 884-X01 ABS
TOYOLAC® 900-352 ABS
TOYOLAC® 910 X01 ABS
TOYOLAC® 912 X01 ABS
TOYOLAC® 920 555 ABS
TOYOLAC® 930-355 ABS
TOYOLAC® ASG-10 SAN-GF10
TOYOLAC® ASG-20 SAN-GF20
TOYOLAC® ASG-30 SAN-GF30
TOYOLAC® ASG-40 SAN-GF40
TOYOLAC® AX05 X03 ABS
TOYOLAC® PX10-X06 (ABS+PC)
TOYOLAC® SX01 (ABS+PA6)
TOYOLAC® TP10 ABS
TOYOLAC® TP82-X05 ABS
TOYOLAC® TP88 ABS
TOYOLAC® TP90 ABS
TOYOLAC® 100G-23R ABS-(GF+GS)23
TOYOLAC® 100G-30R ABS-(GF+GS)30
TOYOLAC® 125-X82 ABS
TOYOLAC® 300-325 ABS
TOYOLAC® 335-X01 ABS
TOYOLAC® 440Y-X01 ABS
TOYOLAC® 470Y-TG1 ABS
TOYOLAC® 520-X17 ABS
TOYOLAC® 530-X01 ABS
TOYOLAC® 550R-T25 ABS-(GF+MD)25
TOYOLAC® 600-X06 ABS
TOYOLAC® 910-X15 ABS
TOYOLAC® 950-X01 ABS
TOYOLAC® 982-X02 ABS
TOYOLAC® A20C-300 ABS
TOYOLAC® A25C-300 ABS
TOYOLAC® AX05-X06 ABS
TOYOLAC® AX05-X08 ABS
TOYOLAC® AX05-X38 ABS
TOYOLAC® PX10-X07 (ABS+PC)
TOYOLAC® SX10G-15 (ABS+PA6)-GF15
TOYOLAC® TM335-GM1 ABS
TOYOLAC® TM335-GM2 ABS
TOYOLAC® TP10-GP1 ABS
TOYOLAC® TP50-X03 (ABS+PC)
TOYOLAC® TP60-X02 ABS
TOYOLAC® TP70 ABS
TOYOLAC® TP86F-X01 ABS
TOYOLAC® TP90-X10 ABS
TOYOLAC® VX10G20 (ABS+PBT)-GF20
TOYOLAC® VX10-X01 (ABS+PBT)
TOYOLAC® 420Y MH1 ABS
TOYOLAC® 430Y MH1 ABS
TOYOLAC® 900 352A ABS

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.