Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Titanvene™ LL0209AA - (PE-LLD) - PT. Titan Kimia Nusantara Tbk.

Material Data Center offers the following functions for Titanvene™ LL0209AA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Titanvene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Rheological propertiesValueUnitTest Standard
ISO Data
Melt flow index, MFI 1 g/10min ISO 1133
MFI temperature 190 °C -
MFI load 2.16 kg -
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 122 °C ISO 11357-1/-3
Other propertiesValueUnitTest Standard
ISO Data
Density 920 kg/m³ ISO 1183
Film PropertiesValueUnitTest Standard
ISO Data
Stress at yield, parallel 11 MPa ISO 527-3
Stress at yield, normal 12 MPa ISO 527-3
Maximum strain, parallel 800 % ISO 527-3
Maximum strain, normal 900 % ISO 527-3
Dart drop A 120 g ISO 7765-1
Optical propertiesValueUnitTest Standard
ASTM Data
Gloss 50 - ASTM D 2457
Haze 15 % ASTM D 1003
Characteristics
Processing
Blown Film Extrusion
Additives
Antiblocking agent
Special Characteristics
Transparent
Certifications
Food contact, Food approval 1935/2004/EC, Food approval FDA 21 CFR
Applications
Packaging
Regional Availability
Asia Pacific
Disclaimer
Copyright M-Base Engineering+Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from M-Base; this is especially valid for claims of compensation resulting from consequential damages. M-Base explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: 2017-09-22 Source: www.materialdatacenter.com