Tradename: Titanvene
Family: PE-HD, PE-LLD
Producer: PT. Titan Kimia Nusantara Tbk
23 hits in the material database

Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Titanvene™ BPD3220 (PE-LLD)
Titanvene™ HD3840UA (PE-MD)
Titanvene™ HD4708AA (PE-HD)
Titanvene™ HD5070P (PE-HD)
Titanvene™ HD5120EA-B (PE-HD)
Titanvene™ HD5120GB-B (PE-HD)
Titanvene™ HD5211EA-B (PE-HD)
Titanvene™ HD5218EA (PE-HD)
Titanvene™ HD5301AA (PE-HD)
Titanvene™ HD5401GA (PE-HD)
Titanvene™ HD5502GA (PE-HD)
Titanvene™ HD5609AA (PE-HD)
Titanvene™ HD5707GM (PE-HD)
Titanvene™ HD5740UA (PE-HD)
Titanvene™ HD6070EA (PE-HD)
Titanvene™ HD6070UA (PE-HD)
Titanvene™ HM4560UA (PE-HD)
Titanvene™ HM5250UA (PE-HD)
Titanvene™ HM5420GA (PE-HD)
Titanvene™ LL0209AA (PE-LLD)
Titanvene™ LL0209SR (PE-LLD)
Titanvene™ LL0220AA (PE-LLD)
Titanvene™ LL0220SR (PE-LLD)

Additional information about this tradename, like producer contact address, etc. can be found at For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.