Processing/Physical Characteristics | Value | Unit | Test Standard |
ISO Data |
Melt flow index, MFI |
4 |
g/10min |
ISO 1133 |
Temperature |
190 |
°C |
- |
Load |
2.16 |
kg |
- |
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Shore D hardness |
48 |
- |
ISO 7619-1 |
Thermal properties | Value | Unit | Test Standard |
ISO Data |
Vicat softening temperature, A |
92 |
°C |
ISO 306 |
Optical properties | Value | Unit | Test Standard |
ISO Data |
Haze |
8 |
- |
ISO 14782 |
Other properties | Value | Unit | Test Standard |
Density |
922 |
kg/m³ |
ISO 1183 |
Film Properties | Value | Unit | Test Standard |
ISO Data |
Maximum stress, parallel |
22 |
MPa |
ISO 527-3 |
Maximum stress, normal |
16 |
MPa |
ISO 527-3 |
Maximum strain, parallel |
390 |
% |
ISO 527-3 |
Maximum strain, normal |
590 |
% |
ISO 527-3 |
Dart drop A |
80 |
g |
ISO 7765-1 |
Type of extrusion |
blown |
- |
- |
Thickness of specimen |
0.04 |
mm |
- |
Processing Recommendation Injection Molding | Value | Unit | Test Standard |
Melt temperature |
170 - 190 |
°C |
- |
Processing Recommendation Extrusion | Value | Unit | Test Standard |
Melt temperature |
150 - 190 |
°C |
- |
Characteristics
Processing
Injection Molding, Blown Film Extrusion, Film Extrusion
Delivery form
Pellets
Special Characteristics
Transparent
Certifications
Food contact, Food approval 1935/2004/EC, Food approval 10/2011, Food approval FDA 21 CFR, RoHS compliant
Applications
Electrical and Electronical, Medical, Packaging, Toys
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.