Processing/Physical Characteristics | Value | Unit | Test Standard |
Other Standards[S] |
Melt Flow Index, MFI |
7 |
g/10min |
ASTM D 3307 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Mechanical properties | Value | Unit | Test Standard |
ASTM Data |
Flexural Modulus |
600 |
MPa |
ASTM D 790 |
Shore D Hardness |
55 |
- |
ASTM D 2240 |
Other Standards[S] |
Tensile Strength |
28 |
MPa |
ASTM D 3307 |
Elongation at Break |
290 |
% |
ASTM D 3307 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Thermal properties | Value | Unit | Test Standard |
ASTM Data |
UL 94 Flame rating |
V-0 |
- |
UL 94 |
Limiting Oxygen Index |
95 |
% |
ASTM D 2863 |
Other Standards[S] |
Melting Temperature |
290 |
°C |
ASTM D 4591 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Electrical properties | Value | Unit | Test Standard |
ASTM Data |
Dielectric Strength, Short Time |
80 |
kV/mm |
ASTM D 149 |
Dissipation Factor, 1 MHz |
0.0002 |
- |
ASTM D 150 |
Dielectric Constant, 1 MHz |
2.03 |
- |
ASTM D 150 |
Volume Resistivity |
1E18 |
Ohm*cm |
ASTM D 257 |
Other properties | Value | Unit | Test Standard |
Water Absorption, 24hr |
0.03 |
% |
ASTM D 570 |
Density |
2150 |
kg/m³ |
ASTM D 792 |
Characteristics
Processing
Injection Molding, Pipe/Tube Extrusion, Other Extrusion, Transfer Molding, Compression Molding
Delivery form
Pellets
Special Characteristics
U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Features
Good Drawdown, Low Smoke, Melt Strength, Thermal Stability, Tribologic Grade
Chemical Resistance
General Chemical Resistance, Environmental Stress Crack Resistance
Certifications
Food contact, Food approval FDA 21 CFR
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com