Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TARFLON® A2500 - PC - Idemitsu Chemicals

Material Data Center offers the following functions for TARFLON® A2500:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tarflon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt flow index, MFI 8 g/10min ISO 1133
Temperature 300 °C -
Load 1.2 kg -
ASTM Data
Mold Shrinkage, MD 0.006 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2000 MPa ISO 527
Yield stress 65 MPa ISO 527
Nominal strain at break >50 % ISO 527
Stress at break 65 MPa ISO 527
Flexural modulus, 23°C 2300 MPa ISO 178
Charpy notched impact strength, +23°C 80 kJ/m² ISO 179/1eA
Rockwell hardness R 120 - ISO 2039-2
ASTM Data
Taber Abrasion Resistance 12 mg/1000 cycles ASTM D 1044
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 125 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 137 °C ISO 75-1/-2
Burning behav. at 1.5 mm nom. thickn. V-2 class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning behav. at thickness h HB class IEC 60695-11-10
Thickness tested 1.9 mm -
Yellow Card available yes - -
ASTM Data
Coefficient of Thermal Expansion, MD 65 E-6/K ASTM D 696
Limiting Oxygen Index 27 % ASTM D 2863
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 2.85 - IEC 62631-2-1
Dissipation factor, 1MHz 92 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Electric strength 30 kV/mm IEC 60243-1
ASTM Data
Arc Resistance 110 s ASTM D 495
Optical propertiesValueUnitTest Standard
ISO Data
Luminous transmittance 87 % ISO 13468-1, -2
Other propertiesValueUnitTest Standard
Density 1200 kg/m³ ISO 1183
Characteristics
Delivery form
Pellets
Special Characteristics
Transparent
Regional Availability
North America, Europe, Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.