Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PC Resin PC2200 - Europe - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PC Resin PC2200 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It is available exclusively at www.sabicpc.com.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 21 cm³/10min ISO 1133
Temperature 300 °C -
Load 1.2 kg -
ASTM Data
Melt Flow Index, MFI 22 g/10min ASTM D 1238
Temperature 300 °C -
Load 1.2 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2350 MPa ISO 527
Yield stress 63 MPa ISO 527
Yield strain 6 % ISO 527
Strain at break 50 % ISO 527
Flexural modulus 2300 MPa ISO 178
Rockwell hardness R 120 - ISO 2039-2
ASTM Data
Tensile Modulus 2350 MPa ASTM D 638
Tensile Strength at Yield 63 MPa ASTM D 638
Elongation at Yield 6 % ASTM D 638
Elongation at Break 70 % ASTM D 638
Flexural Modulus 2300 MPa ASTM D 790
Rockwell Hardness R 120 - ASTM D 785
Izod Impact notched, 1/8 in 640 J/m ASTM D 256
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 122 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 133 °C ISO 75-1/-2
Vicat softening temperature, B 140 °C ISO 306
Burning behav. at 1.5 mm nom. thickn. V-2 class IEC 60695-11-10
Thickness tested 1.5 mm -
Thermal Conductivity 0.2 W/(m K) DIN 52616
ASTM Data
DTUL @ 66 psi 133 °C ASTM D 648
DTUL @ 264 psi 122 °C ASTM D 648
Vicat Temperature 140 °C ASTM D 1525
Thermal Conductivity, solid state 0.0288 W/(m K) ASTM C 177
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 3 - IEC 62631-2-1
Dissipation factor, 100Hz 10 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 100 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Electric strength 27 kV/mm IEC 60243-1
ASTM Data
Dielectric Strength, Short Time 27 kV/mm ASTM D 149
Dissipation Factor, 60 Hz 0.001 - ASTM D 150
Dissipation Factor, 1 MHz 0.01 - ASTM D 150
Dielectric Constant, 60 Hz 3 - ASTM D 150
Dielectric Constant, 1 MHz 3 - ASTM D 150
Volume Resistivity 1E15 Ohm*cm ASTM D 257
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 0.8 % ASTM D 1003
Light Transmittance 90 % ASTM D 1003
Index of Refraction 1.59 - ASTM D 542
Other propertiesValueUnitTest Standard
Water absorption 0.35 % Sim. to ISO 62
Density 1200 kg/m³ ISO 1183
Water Absorption, Equilibrium 0.35 % ASTM D 570
Density 1200 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature ≤120 °C -
Pre-drying - Time 2 - 4 h -
Melt temperature 280 - 300 °C -
Mold temperature 80 - 100 °C -
Zone 1 260 - 280 °C -
Zone 2 270 - 290 °C -
Zone 3 280 - 300 °C -
Nozzle temperature 270 - 290 °C -
Characteristics
Special Characteristics
U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com