Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LLDPE 318B - (PE-LLD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LLDPE 318B:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
SABIC® LLDPE318B is a standard C4-LLDPE grade with a relatively low melt flow rate. SABIC® LLDPE318B is a general grade, typically used for low filled or additive masterbatches in film and blow moulding applications(e.g. slip agents, anti fog agents, anti static agents, thermal stabilizers). This product is not intended for and must not be used in any pharmaceutical/medical applications.
Mechanical propertiesValueUnitTest Standard
ISO Data
Shore D hardness 48 - ISO 7619-1
ASTM Data
Tensile Strength at Yield 12 MPa ASTM D 638
Tensile Strength at Break 13 MPa ASTM D 638
Elongation at Yield 16 % ASTM D 638
Elongation at Break 710 % ASTM D 638
Thermal propertiesValueUnitTest Standard
ISO Data
Vicat softening temperature, A 102 °C ISO 306
Electrical propertiesValueUnitTest Standard
ASTM Data
Dissipation Factor, 60 Hz 0.0005 - ASTM D 150
Dielectric Constant, 60 Hz 2.2 - ASTM D 150
Volume Resistivity >1E15 Ohm*cm ASTM D 257
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 2.1 % ASTM D 1003
Film PropertiesValueUnitTest Standard
ISO Data
Trouser Tear resistance, normal 140 N/mm ISO 6383-1
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com