Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC LDPE 1808AN00 - (PE-LD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC LDPE 1808AN00:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
 
Any use of this information falls under the rules of our disclaimer.
Rheological propertiesValueUnitTest Standard
ISO Data
Melt volume-flow rate (MVR) 33 cm³/10min ISO 1133
Temperature 190 °C ISO 1133
Load 5 kg ISO 1133
Melt flow index (MFI) 25 g/10min ISO 1133
MFI temperature 190 °C ISO 1133
MFI load 5 kg ISO 1133
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 160 MPa ISO 527-1/-2
Yield stress 8 MPa ISO 527-1/-2
Stress at break 12 MPa ISO 527-1/-2
Strain at break >50 % ISO 527-1/-2
Tensile creep modulus (1h) 80 MPa ISO 899-1
Tensile creep modulus (1000h) 50 MPa ISO 899-1
Izod Impact notched (23°C) 45 kJ/m² ISO 180/1A
Izod Impact notched 7 kJ/m² ISO 180/1A
Temperature -30 °C ISO 180/1A
Shore D hardness (15s) 46 - ISO 868
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature (10°C/min) 107 °C ISO 11357-1/-3
Temp. of deflection under load (0.45 MPa) 40 °C ISO 75-1/-2
Other propertiesValueUnitTest Standard
ISO Data
Density 920 kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Powder
Chemical Resistance
Environmental Stress Crack Resistance
Regional Availability
North America, Europe, Asia Pacific, South and Central America, Near East/Africa
Disclaimer
Copyright M-Base Engineering+Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from M-Base; this is especially valid for claims of compensation resulting from consequential damages. M-Base explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: 2014-04-24 Source: www.materialdatacenter.com