Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® PP 515A - PP - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® PP 515A:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Product Texts
SABIC® PP 515A is characterized by high flow and broad molecular weight distribution. It contains an anti gas fading stabilisation package.Application: SABIC® PP 515A is suitable for (bulked) continuous filaments, including mono and tri colour carpet yarns.Health, Safety and Food Contact regulations: Material Safety Data Sheets (MSDS) and Product Safety declarations are available on our Internet site
http://www.SABIC.com The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications.This grade material is UL registered under File E111275 (www.ul.com)IMDS 7172624
Mechanical properties | Value | Unit | Test Standard |
ISO Data |
Tensile Modulus |
1700 |
MPa |
ISO 527 |
Yield stress |
37 |
MPa |
ISO 527 |
Yield strain |
8 |
% |
ISO 527 |
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.