Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Repol SRM100NC - PP - Reliance Polymers

Material Data Center offers the following functions for Repol SRM100NC:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Repol datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index 12 g/10min ASTM D 1238
Temperature 230 °C -
Load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 30 MPa ASTM D 638
Elongation at Yield 12 % ASTM D 638
Izod Impact notched, 1/8 in 0.065 kJ/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
DTUL @ 66 psi 95 °C ASTM D 648
Melting Temperature 150 °C ASTM D 3418
Characteristics
Processing
Injection Molding, Blow Molding
Special Characteristics
Anti-static
Features
Copolymer, Random Copolymer
Certifications
Food contact, Food approval FDA 21 CFR
Regional Availability
Europe, Asia Pacific, Near East/Africa
Disclaimer
Copyright M-Base Engineering+Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from M-Base; this is especially valid for claims of compensation resulting from consequential damages. M-Base explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: 2017-09-22 Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.