Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin PX0844 - Asia - (PPE+PS) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin PX0844 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
NORYL™ PX0844 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This grade exhibits very low moisture absorption, hydrolytic stability, dimensional stabilty, good foam adhesion, and property retention over a wide temperature range. NORYL PX0844 resin is inherently UL94 HB and is an excellent candidate for automotive interior applications such as instrument panels, audio components, speaker housings, and interior trim. *see NORYL PX0888 resin for higher heat resistance.
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 49 MPa ASTM D 638
Elongation at Break 30 % ASTM D 638
Rockwell Hardness R 114 - ASTM D 785
Izod Impact notched, 1/8 in 234 J/m ASTM D 256
Izod Impact notched, Low-Temperature 133 J/m ASTM D 256
Temperature -40 °C -
Other propertiesValueUnitTest Standard
Density 1060 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 105 - 110 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 275 - 305 °C -
Mold temperature 70 - 100 °C -
Zone 1 245 - 295 °C -
Zone 2 255 - 300 °C -
Zone 3 265 - 305 °C -
Screw speed 20 - 100 rpm -
Back pressure 0.3 - 0.7 MPa -
Characteristics
Processing
Injection Molding
Chemical Resistance
Hydrolytically Stable
Applications
Automotive
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.