Any use of this information falls under the rules of our
disclaimer.
Processing/Physical Characteristics | Value | Unit | Test Standard |
ASTM Data |
Melt Flow Index, MFI |
7 |
g/10min |
ASTM D 1238 |
Temperature |
300 |
°C |
- |
Load |
1.2 |
kg |
- |
Mold Shrinkage, MD |
0.006 |
mm/mm |
ASTM D 955 |
Mechanical properties | Value | Unit | Test Standard |
ASTM Data |
Tensile Modulus |
2410 |
MPa |
ASTM D 638 |
Tensile Strength at Yield |
60 |
MPa |
ASTM D 638 |
Tensile Strength at Break |
72 |
MPa |
ASTM D 638 |
Elongation at Yield |
6 |
% |
ASTM D 638 |
Elongation at Break |
150 |
% |
ASTM D 638 |
Flexural Modulus |
2410 |
MPa |
ASTM D 790 |
Flexural Strength |
96 |
MPa |
ASTM D 790 |
Rockwell Hardness |
M 74 |
- |
ASTM D 785 |
Izod Impact notched, 1/8 in |
900 |
J/m |
ASTM D 256 |
Izod Impact unnotched, 1/8 in |
N |
J/m |
ASTM D 256 |
Thermal properties | Value | Unit | Test Standard |
ISO Data |
Burning behav. at thickness h |
HB |
class |
IEC 60695-11-10 |
Thickness tested |
3.0 |
mm |
- |
Yellow Card available |
yes |
- |
- |
Glow Wire Ignition Temperature (GWIT) |
850 |
°C |
IEC 60695-2-13 |
GWIT - thickness tested (1) |
2 |
mm |
- |
ASTM Data |
UL 94 Flame rating |
HB |
- |
UL 94 |
Thickness tested |
0.5 |
mm |
- |
Coefficient of Thermal Expansion, MD |
68 |
E-6/K |
ASTM D 696 |
DTUL @ 66 psi |
145[ann.] |
°C |
ASTM D 648 |
DTUL @ 264 psi |
129 |
°C |
ASTM D 648 |
Vicat Temperature |
151 |
°C |
ASTM D 1525 |
Limiting Oxygen Index |
26 |
% |
ASTM D 2863 |
Electrical properties | Value | Unit | Test Standard |
ISO Data |
Comparative tracking index |
250 |
- |
IEC 60112 |
ASTM Data |
Dielectric Strength, Short Time |
17 |
kV/mm |
ASTM D 149 |
Dissipation Factor, 60 Hz |
0.001 |
- |
ASTM D 150 |
Dielectric Constant, 60 Hz |
3 |
- |
ASTM D 150 |
Volume Resistivity |
2E17 |
Ohm*cm |
ASTM D 257 |
Optical properties | Value | Unit | Test Standard |
ASTM Data |
Haze |
1.1 |
% |
ASTM D 1003 |
Light Transmittance |
89 |
% |
ASTM D 1003 |
Index of Refraction |
1.59 |
- |
ASTM D 542 |
Other properties | Value | Unit | Test Standard |
Water Absorption, 24hr |
0.15 |
% |
ASTM D 570 |
Water Absorption, Equilibrium |
0.32 |
% |
ASTM D 570 |
Density |
1200 |
kg/m³ |
ASTM D 792 |
Characteristics
Processing
Injection Molding, Sheet Extrusion, Other Extrusion
Additives
Release agent
Special Characteristics
High impact or impact modified, U.V. stabilized or stable to weather, Heat stabilized or stable to heat, Transparent
Regional Availability
North America, Europe, Asia Pacific, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com