Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Lexan EXL1132T - PC - SABIC Innovative Plastics

Material Data Center offers the following functions for Lexan EXL1132T:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index 20 g/10min ASTM D 1238
Mold Shrinkage, MD 0.006 mm/mm ASTM D 955
Mold Shrinkage, TD 0.006 mm/mm ASTM D 955
Density 1190 kg/m³ ASTM D 792
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Modulus 2261.48 MPa ASTM D 638
Tensile Strength at Yield 57.9 MPa ASTM D 638
Tensile Strength at Break 56.5 MPa ASTM D 638
Elongation at Yield 5.7 % ASTM D 638
Elongation at Break 118 % ASTM D 638
Flexural Modulus 2247.69 MPa ASTM D 790
Flexural Strength 94.5 MPa ASTM D 790
Izod Impact notched, 1/8 in 0.731 kJ/m ASTM D 256
Izod Impact notched, Low-Temperature 0.614 kJ/m ASTM D 256
Temperature -30 °C -
Thermal propertiesValueUnitTest Standard
ASTM Data
UL 94 Flame rating HB - UL 94
Thickness tested 1.5 mm -
Coefficient of Thermal Expansion, MD 74.7 E-6/K ASTM D 696
Coefficient of Thermal Expansion, TD 76.3 E-6/K ASTM D 696
DTUL @ 264 psi 122 °C ASTM D 648
Vicat Temperature 138 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ASTM Data
Surface Resistivity 1E15 Ohm ASTM D 257
Volume Resistivity 1E15 Ohm*cm ASTM D 257
Optical propertiesValueUnitTest Standard
ASTM Data
Haze 3 % ASTM D 1003
Light Transmittance 82 % ASTM D 1003
Characteristics
Processing
Injection Molding
Special Characteristics
U.V. stabilized or stable to weather, Transparent
Features
Copolymer
Applications
General Purpose
Regional Availability
North America
Disclaimer
Copyright M-Base Engineering+Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from M-Base; this is especially valid for claims of compensation resulting from consequential damages. M-Base explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: 2017-01-20 Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.