Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ VISUALFX™ Resin FXM141R Asia - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ VISUALFX™ Resin FXM141R Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
FXM141R is a LEXAN PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect properties, Application testing always reccomended.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 11 cm³/10min ISO 1133
Temperature 300 °C -
Load 1.2 kg -
ASTM Data
Melt Flow Index, MFI 10.8 g/10min ASTM D 1238
Temperature 300 °C -
Load 1.2 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2350 MPa ISO 527
Yield stress 63 MPa ISO 527
Yield strain 6 % ISO 527
Stress at break 55 MPa ISO 527
Strain at break 50 % ISO 527
Flexural modulus, 23°C 2300 MPa ISO 178
Charpy impact strength, +23°C N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 12 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 13 kJ/m² ISO 179/1eA
Izod impact strength, +23°C N kJ/m² ISO 180/1U
Izod notched impact strength, +23°C 10 kJ/m² ISO 180/1A
Izod notched impact strength 8 kJ/m² ISO 180/1A
Temperature -30 °C -
Ball indentation hardness 95 MPa ISO 2039-1
ASTM Data
Tensile Modulus 2340 MPa ASTM D 638
Tensile Strength at Yield 62 MPa ASTM D 638
Tensile Strength at Break 55 MPa ASTM D 638
Elongation at Yield 6.2 % ASTM D 638
Elongation at Break 90 % ASTM D 638
Flexural Modulus 2340 MPa ASTM D 790
Izod Impact notched, 1/8 in 214 J/m ASTM D 256
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 125 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 136 °C ISO 75-1/-2
Vicat softening temperature, B 141 °C ISO 306
Coeff. of linear therm. expansion, parallel 69.6 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 70.6 E-6/K ISO 11359-1/-2
Burning behav. at thickness h HB class IEC 60695-11-10
Thickness tested 0.7 mm -
Yellow Card available yes - -
ASTM Data
Coefficient of Thermal Expansion, MD 68.7 E-6/K ASTM D 696
Coefficient of Thermal Expansion, TD 69.5 E-6/K ASTM D 696
DTUL @ 66 psi 138 °C ASTM D 648
DTUL @ 264 psi 127 °C ASTM D 648
Vicat Temperature 154 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ISO Data
Comparative tracking index 212 - IEC 60112
Other propertiesValueUnitTest Standard
Water absorption 0.35 % Sim. to ISO 62
Humidity absorption 0.15 % Sim. to ISO 62
Density 1200 kg/m³ ISO 1183
Density 1200 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 295 - 315 °C -
Mold temperature 70 - 95 °C -
Zone 1 270 - 295 °C -
Zone 2 280 - 305 °C -
Zone 3 295 - 315 °C -
Nozzle temperature 290 - 310 °C -
Screw speed 40 - 70 rpm -
Back pressure 0.3 - 0.7 MPa -
Characteristics
Processing
Injection Molding
Features
Metallic effect
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.