Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ VISUALFX™ Resin FXG1414T - Asia - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ VISUALFX™ Resin FXG1414T - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.

UL Yellow Card Link E207780-512794
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 9 cm³/10min ISO 1133
Temperature 300 °C -
Load 1.2 kg -
ASTM Data
Melt Flow Index, MFI 10 g/10min ASTM D 1238
Temperature 300 °C -
Load 1.2 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2250 MPa ISO 527
Yield stress 56 MPa ISO 527
Yield strain 5.4 % ISO 527
Stress at break 49 MPa ISO 527
Strain at break 11.3 % ISO 527
Flexural modulus 2150 MPa ISO 178
Charpy notched impact strength, +23°C 45 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C, 4mm 32 kJ/m² ISO 180/1A
Izod notched impact strength, -30°C, 4mm 19 kJ/m² ISO 180/1A
ASTM Data
Tensile Modulus 2060 MPa ASTM D 638
Tensile Strength at Yield 58 MPa ASTM D 638
Tensile Strength at Break 45 MPa ASTM D 638
Elongation at Yield 5.7 % ASTM D 638
Elongation at Break 52 % ASTM D 638
Flexural Modulus 2230 MPa ASTM D 790
Izod Impact notched, 1/8 in 523 J/m ASTM D 256
Izod Impact notched, Low-Temperature 347 J/m ASTM D 256
Temperature -30 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 117 °C ISO 75-1/-2
Vicat softening temperature, B 139 °C ISO 306
Vicat softening temperature, 120°C/h 50N 142 °C ISO 306
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
DTUL @ 264 psi 121 °C ASTM D 648
Vicat Temperature 139 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Water absorption 0.13 % Sim. to ISO 62
Humidity absorption 0.09 % Sim. to ISO 62
Density 1180 kg/m³ ISO 1183
Density 1180 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 295 - 315 °C -
Mold temperature 70 - 95 °C -
Zone 1 270 - 295 °C -
Zone 2 280 - 305 °C -
Zone 3 295 - 315 °C -
Screw speed 40 - 70 rpm -
Back pressure 0.3 - 0.7 MPa -
Characteristics
Processing
Injection Molding
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.