Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ VISUALFX™ Resin FXD153 Americas - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ VISUALFX™ Resin FXD153 Americas:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
FXD153 is an Extrusion / Blow molding grade in a Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect properties, Application testing always reccomended.
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 2.5 g/10min ASTM D 1238
Temperature 300 °C -
Load 1.2 kg -
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Modulus 2340 MPa ASTM D 638
Tensile Strength at Yield 62 MPa ASTM D 638
Tensile Strength at Break 66 MPa ASTM D 638
Elongation at Yield 7 % ASTM D 638
Elongation at Break 110 % ASTM D 638
Flexural Modulus 2340 MPa ASTM D 790
Izod Impact notched, 1/8 in 748 J/m ASTM D 256
Izod Impact unnotched, 1/8 in 3200 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ASTM Data
Coefficient of Thermal Expansion, MD 68 E-6/K ASTM D 696
DTUL @ 66 psi 138 °C ASTM D 648
DTUL @ 264 psi 132 °C ASTM D 648
Vicat Temperature 157 °C ASTM D 1525
Other propertiesValueUnitTest Standard
Density 1200 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 320 - 345 °C -
Mold temperature 80 - 115 °C -
Zone 1 300 - 320 °C -
Zone 2 310 - 330 °C -
Zone 3 320 - 345 °C -
Nozzle temperature 315 - 340 °C -
Screw speed 40 - 70 rpm -
Back pressure 0.3 - 0.7 MPa -
Processing Recommendation ExtrusionValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 265 - 280 °C -
Mold temperature 60 - 100 °C -
Zone 1 260 - 290 °C -
Zone 2 260 - 290 °C -
Zone 3 260 - 290 °C -
Zone 4 260 - 290 °C -
Zone 5 260 - 290 °C -
Characteristics
Processing
Injection Molding, Other Extrusion, Blow Molding
Features
Light Diffusing
Applications
Aircraft and Aerospace, Automotive, Electrical and Electronical
Regional Availability
North America, South and Central America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.