Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer HPH4504 - Europe - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer HPH4504 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam sterilizable.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 12 cm³/10min ISO 1133
Temperature 330 °C -
Load 2.16 kg -
ASTM Data
Melt Flow Index, MFI 3 g/10min ASTM D 1238
Temperature 300 °C -
Load 1.2 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2260 MPa ISO 527
Yield stress 65 MPa ISO 527
Yield strain 7 % ISO 527
Stress at break 65 MPa ISO 527
Strain at break 50 % ISO 527
Flexural modulus 2120 MPa ISO 178
Charpy notched impact strength, +23°C 15 kJ/m² ISO 179/1eA
Izod notched impact strength, +23°C, 4mm 13 kJ/m² ISO 180/1A
Izod notched impact strength, -30°C, 4mm 11 kJ/m² ISO 180/1A
ASTM Data
Tensile Modulus 2090 MPa ASTM D 638
Tensile Strength at Yield 65 MPa ASTM D 638
Tensile Strength at Break 71 MPa ASTM D 638
Elongation at Yield 7 % ASTM D 638
Elongation at Break 122 % ASTM D 638
Flexural Modulus 2020 MPa ASTM D 790
Rockwell Hardness R 122 - ASTM D 785
Izod Impact notched, 1/8 in 640 J/m ASTM D 256
Izod Impact notched, Low-Temperature 144 J/m ASTM D 256
Temperature -30 °C -
Izod Impact unnotched, 1/8 in 3200 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 132 °C ISO 75-1/-2
Vicat softening temperature, B 154 °C ISO 306
Vicat softening temperature, 120°C/h 50N 155 °C ISO 306
ASTM Data
DTUL @ 264 psi 143 °C ASTM D 648
Vicat Temperature 160 °C ASTM D 1525
Thermal Conductivity, solid state 0.0303 W/(m K) ASTM C 177
Specific Heat 1260 J/(kg K) ASTM C 351
Electrical propertiesValueUnitTest Standard
ASTM Data
Dissipation Factor, 60 Hz 0.0012 - ASTM D 150
Dielectric Constant, 60 Hz 3.15 - ASTM D 150
Dielectric Constant, 1 MHz 3 - ASTM D 150
Volume Resistivity >1E15 Ohm*cm ASTM D 257
Other propertiesValueUnitTest Standard
Water absorption 0.16 % Sim. to ISO 62
Humidity absorption 0.35 % Sim. to ISO 62
Density 1200 kg/m³ ISO 1183
Density 1200 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 340 - 360 °C -
Mold temperature 80 - 115 °C -
Zone 1 315 - 340 °C -
Zone 2 325 - 350 °C -
Zone 3 340 - 360 °C -
Screw speed 40 - 70 rpm -
Back pressure 0.3 - 0.7 MPa -
Characteristics
Processing
Injection Molding
Special Characteristics
Ethylene Oxide (EtO) Sterilization, Steam sterilization, Gamma irradiation sterilization, Electron beam (e-beam) sterilization
Certifications
US Pharmacopeia Class VI Approved
Applications
Medical
Regional Availability
Europe
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.