Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer EXL9330 - Americas - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer EXL9330 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
EXL9330 is an opaque (PC)- siloxane copolymer resin that offers extreme low temperature (-60 C) ductility in combination with excellent processability. This UV stabilized, medium flow resin features UL f1/V-0/5VA rating with non-chlorinated, non-brominated flame retardant agents for wide range of colors. EXL9330 is an excellent candidate for a broad range of applications such as mobile phones, tablets, industrial housings, electric circuit protection, personal safety helmets, electric vehicle supply equipment (EVSE) housings and connectors.

UL Yellow Card Link E121562-220779
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 9 cm³/10min ISO 1133
Temperature 300 °C -
Load 1.2 kg -
ASTM Data
Melt Flow Index, MFI 10 g/10min ASTM D 1238
Temperature 300 °C -
Load 1.2 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2100 MPa ISO 527
Yield stress 55 MPa ISO 527
Yield strain 6 % ISO 527
Stress at break 60 MPa ISO 527
Strain at break 50 % ISO 527
Flexural modulus 2200 MPa ISO 178
Charpy impact strength, +23°C, 3mm N kJ/m² ISO 179/1eU
Charpy impact strength, -30°C, 3mm N kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C, 3mm 75 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C, 3mm 60 kJ/m² ISO 179/1eA
Izod impact strength, +23°C N kJ/m² ISO 180/1U
Izod notched impact strength, +23°C, 3mm 70 kJ/m² ISO 180/1A
Izod notched impact strength, -30°C, 3mm 55 kJ/m² ISO 180/1A
Ball indentation hardness 90 MPa ISO 2039-1
ASTM Data
Tensile Modulus 2100 MPa ASTM D 638
Tensile Strength at Yield 58 MPa ASTM D 638
Tensile Strength at Break 61 MPa ASTM D 638
Elongation at Yield 6 % ASTM D 638
Elongation at Break 130 % ASTM D 638
Flexural Modulus 2060 MPa ASTM D 790
Izod Impact notched, 1/8 in 801 J/m ASTM D 256
Izod Impact notched, 1/4 in 640 J/m ASTM D 256
Izod Impact notched, Low-Temperature 678 J/m ASTM D 256
Temperature -30 °C -
Thermal propertiesValueUnitTest Standard
ISO Data
Vicat softening temperature, B 140 °C ISO 306
Vicat softening temperature, 120°C/h 50N 142 °C ISO 306
Burning behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning behav. at thickness h V-1 class IEC 60695-11-10
Thickness tested 0.8 mm -
Burning behav. 5V at thickness h 5VB class IEC 60695-11-20
Thickness tested 2.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 825 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 825 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 mm -
Glow Wire Ignition Temperature (GWIT) 825 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
DTUL @ 66 psi 134 °C ASTM D 648
DTUL @ 264 psi 120 °C ASTM D 648
Vicat Temperature 142 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 1MHz 2.7 - IEC 62631-2-1
Dissipation factor, 1MHz 85 E-4 IEC 62631-2-1
Volume resistivity >1E13 Ohm*m IEC 62631-3-1
Surface resistivity >1E15 Ohm IEC 62631-3-2
Comparative tracking index 225 - IEC 60112
ASTM Data
Dielectric Strength, Short Time 17 kV/mm ASTM D 149
Dissipation Factor, 60 Hz 0.0024 - ASTM D 150
Dissipation Factor, 1 MHz 0.0085 - ASTM D 150
Dielectric Constant, 60 Hz 2.95 - ASTM D 150
Dielectric Constant, 1 MHz 2.9 - ASTM D 150
Other propertiesValueUnitTest Standard
Water absorption 0.35 % Sim. to ISO 62
Humidity absorption 0.15 % Sim. to ISO 62
Density 1190 kg/m³ ISO 1183
Density 1180 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 255 - 315 °C -
Mold temperature 70 - 95 °C -
Zone 1 235 - 295 °C -
Zone 2 245 - 305 °C -
Zone 3 255 - 315 °C -
Screw speed 40 - 70 rpm -
Back pressure 0.3 - 0.7 MPa -
Characteristics
Processing
Injection Molding
Additives
Flame retarding agent
Special Characteristics
Flame retardant
Applications
Automotive
Regional Availability
North America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.