Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer EXL9111 - Asia - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer EXL9111 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
LEXAN EXL9111 polycarbonate-Siloxane copolymer resin is a high flow, high impact,non-chlorinated, non-brominated flame retardant opaque injection molding (IM) grade.

UL Yellow Card Link E207780-103826700
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 20 g/10min ASTM D 1238
Temperature 300 °C -
Load 1.2 kg -
Mold Shrinkage, MD 0.6 mm/mm ASTM D 955
Mold Shrinkage, TD 0.62 mm/mm ASTM D 955
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2350 MPa ISO 527
Yield stress 60 MPa ISO 527
Yield strain 4.5 % ISO 527
Stress at break 47 MPa ISO 527
Strain at break 46.7 % ISO 527
Flexural modulus 2310 MPa ISO 178
Izod impact strength, +23°C, 4mm N kJ/m² ISO 180/1U
Izod notched impact strength, +23°C, 4mm 51.3 kJ/m² ISO 180/1A
Izod notched impact strength, -30°C, 4mm 104 kJ/m² ISO 180/1A
ASTM Data
Tensile Modulus 2387 MPa ASTM D 638
Tensile Strength at Yield 60 MPa ASTM D 638
Tensile Strength at Break 54 MPa ASTM D 638
Elongation at Yield 4.6 % ASTM D 638
Elongation at Break 76.4 % ASTM D 638
Flexural Modulus 2440 MPa ASTM D 790
Rockwell Hardness L92.2 - ASTM D 785
Izod Impact notched, 1/8 in 753 J/m ASTM D 256
Izod Impact notched, Low-Temperature 124 J/m ASTM D 256
Temperature -30 °C -
Izod Impact unnotched, 1/8 in N J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 103 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 112 °C ISO 75-1/-2
Vicat softening temperature, B 117 °C ISO 306
Vicat softening temperature, 120°C/h 50N 119 °C ISO 306
Burning behav. at thickness h V-1 class IEC 60695-11-10
Thickness tested 0.8 mm -
ASTM Data
DTUL @ 66 psi 111 °C ASTM D 648
DTUL @ 264 psi 101 °C ASTM D 648
Vicat Temperature 126 °C ASTM D 1525
Electrical propertiesValueUnitTest Standard
ASTM Data
Surface Resistivity >1E15 Ohm ASTM D 257
Volume Resistivity >1E15 Ohm*cm ASTM D 257
Other propertiesValueUnitTest Standard
Humidity absorption 0.43 % Sim. to ISO 62
Density 1190 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 100 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 280 - 305 °C -
Mold temperature 60 - 80 °C -
Zone 1 260 - 285 °C -
Zone 2 275 - 295 °C -
Zone 3 280 - 305 °C -
Characteristics
Processing
Injection Molding
Additives
Flame retarding agent
Special Characteristics
Flame retardant
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com