Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer EXL5429S - Asia - PC-GF - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer EXL5429S - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Lexan* EXL5429S polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features (all color rating) UL94 V0 @ 1.5mm flame, RTI(elec.) 130C, based on non-chlorine, non-bromine FR agents with excellent processability and improved release performance. Available in custom opaque colors.

UL Yellow Card Link E45329-103983721
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 15 cm³/10min ISO 1133
Temperature 330 °C -
Load 1.2 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 3600 MPa ISO 527
Yield stress 58 MPa ISO 527
Yield strain 4 % ISO 527
Stress at break 45 MPa ISO 527
Strain at break 7 % ISO 527
Flexural modulus 3300 MPa ISO 178
Charpy impact strength, +23°C, 3mm 90 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C, 3mm 12 kJ/m² ISO 179/1eA
Izod impact strength, +23°C 70 kJ/m² ISO 180/1U
Izod notched impact strength, +23°C, 3mm 10 kJ/m² ISO 180/1A
Izod notched impact strength, -30°C, 3mm 6 kJ/m² ISO 180/1A
ASTM Data
Tensile Modulus 3500 MPa ASTM D 638
Tensile Strength at Yield 57 MPa ASTM D 638
Tensile Strength at Break 45 MPa ASTM D 638
Elongation at Yield 4 % ASTM D 638
Elongation at Break 7 % ASTM D 638
Flexural Modulus 3200 MPa ASTM D 790
Izod Impact notched, 1/8 in 120 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 145 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 154 °C ISO 75-1/-2
Vicat softening temperature, 120°C/h 50N 156 °C ISO 306
Burning behav. at 1.5 mm nom. thickn. V-0 class IEC 60695-11-10
Thickness tested 1.5 mm -
Burning behav. at thickness h V-2 class IEC 60695-11-10
Thickness tested 0.8 mm -
Burning behav. 5V at thickness h 5VB class IEC 60695-11-20
Thickness tested 3.0 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
DTUL @ 66 psi 154 °C ASTM D 648
DTUL @ 264 psi 145 °C ASTM D 648
Electrical propertiesValueUnitTest Standard
ISO Data
Volume resistivity 1E13 Ohm*m IEC 62631-3-1
Comparative tracking index 175 - IEC 60112
Other propertiesValueUnitTest Standard
Density 1260 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 310 - 330 °C -
Mold temperature 80 - 115 °C -
Zone 1 290 - 310 °C -
Zone 2 300 - 320 °C -
Zone 3 310 - 330 °C -
Screw speed 40 - 70 rpm -
Back pressure 0.3 - 0.7 MPa -
Characteristics
Processing
Injection Molding
Additives
Flame retarding agent
Special Characteristics
Flame retardant
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.