Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ Copolymer 4704 - Asia - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ Copolymer 4704 - Asia:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with biocompatibility information and should not be used for medical applications which require biocompatibility. Alternative grade HPH4704.

UL Yellow Card Link E207780-101218623
Processing/Physical CharacteristicsValueUnitTest Standard
ASTM Data
Melt Flow Index, MFI 2 g/10min ASTM D 1238
Temperature 300 °C -
Load 1.2 kg -
Mechanical propertiesValueUnitTest Standard
ASTM Data
Tensile Strength at Yield 65 MPa ASTM D 638
Tensile Strength at Break 77 MPa ASTM D 638
Elongation at Break 78 % ASTM D 638
Flexural Modulus 2330 MPa ASTM D 790
Rockwell Hardness R 127 - ASTM D 785
Izod Impact notched, 1/8 in 373 J/m ASTM D 256
Izod Impact unnotched, 1/8 in 3200 J/m ASTM D 256
Thermal propertiesValueUnitTest Standard
ISO Data
Burning behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.5 mm -
ASTM Data
DTUL @ 264 psi 148 °C ASTM D 648
Thermal Conductivity, solid state 0.0303 W/(m K) ASTM C 177
Specific Heat 1250 J/(kg K) ASTM C 351
Electrical propertiesValueUnitTest Standard
ASTM Data
Dissipation Factor, 60 Hz 0.0016 - ASTM D 150
Dielectric Constant, 60 Hz 3.27 - ASTM D 150
Dielectric Constant, 1 MHz 3.1 - ASTM D 150
Volume Resistivity >1E15 Ohm*cm ASTM D 257
Other propertiesValueUnitTest Standard
Density 1200 kg/m³ ASTM D 792
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 120 °C -
Pre-drying - Time 3 - 4 h -
Processing humidity ≤0.02 % -
Melt temperature 350 - 370 °C -
Mold temperature 80 - 115 °C -
Zone 1 325 - 350 °C -
Zone 2 340 - 360 °C -
Zone 3 350 - 370 °C -
Screw speed 40 - 70 rpm -
Back pressure 0.3 - 0.7 MPa -
Characteristics
Processing
Injection Molding
Certifications
Food contact, Food approval FDA 21 CFR
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.