Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Leona - PA66 - Asahi Kasei Corporation

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Leona" in Material Data Center leads to the following information:

Tradename: Leona
Family: PA66
Producer: Asahi Kasei Corporation
58 hits in the material database
2 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
LEONA™ 1300G PA66-GF33
LEONA™ 1300S PA66
LEONA™ 1302S PA66
LEONA™ 1330G PA66-GF...
LEONA™ 13G15 PA66-GF15
LEONA™ 13G43 PA66-GF43
LEONA™ 13G50 PA66-GF50
LEONA™ 1402G PA66-GF33
LEONA™ 1402S PA66
LEONA™ 14G15 PA66-GF15
LEONA™ 14G25 PA66-GF25
LEONA™ 14G33 PA66-GF33
LEONA™ 14G43 PA66-GF43
LEONA™ 14G50 PA66-GF50
LEONA™ 1500 PA66
LEONA™ 1502S PA66
LEONA™ 1700S PA66
LEONA™ 1702 PA66
LEONA™ 53G33 (PA66+PA612)-GF33
LEONA™ 54G33 (PA66+PA6)-GF33
LEONA™ 54G43 (PA66+PA6)-GF43
LEONA™ 90G33 PA66-GF33
LEONA™ 90G50 PA66-GF50
LEONA™ 90G55 PA66-GF55
LEONA™ 90G60 PA66-GF60
LEONA™ 91G40 PA66-MF
LEONA™ 91G55 PA66-GF
LEONA™ 91G60 PA66-GF
LEONA™ 93G33 (PA6+PA66/6)-GF33
LEONA™ 9400S PA66/6
LEONA™ CR103 PA66-MF
LEONA™ CR301 PA66-MF
LEONA™ CR302 PA66-MF
LEONA™ FG170 PA66-GF15
LEONA™ FG171 PA66-GF
LEONA™ FG172 PA66-GF50
LEONA™ FG173 PA66-GF30
LEONA™ FH772 PA66-GF
LEONA™ FR200 PA66/6
LEONA™ FR370 PA66
LEONA™ MR001 PA66-MF40
LEONA™ TR161 PA66
LEONA™ TR382 PA66
LEONA™ 1502 PA66
LEONA™ 1442 BK PA66
LEONA™ 1542 BK PA66
LEONA™ 14G30 BK PA66-GF30
LEONA™ 14G35 BK PA66-GF35
LEONA™ 14G50 BK PA66-GF50
LEONA™ SG104 BK PA66-GF40
LEONA™ SG105 BK PA66-GF50
LEONA™ SG106 BK PA66-GF60
LEONA™ BG230 PA610-GF
LEONA™ FR650 PA66/6
LEONA™ 14G35 PA66-GF
LEONA™ SH10E PA66-GF
LEONA™ SN103 PA66-GF
LEONA™ SN10B PA66-GF

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.