Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eraclene® MP 90 - (PE-HD) - Versalis S.p.A

Material Data Center offers the following functions for Eraclene® MP 90:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eraclene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Rheological propertiesValueUnitTest Standard
ISO Data
Melt flow index, MFI 7 g/10min ISO 1133
MFI temperature 190 °C -
MFI load 2.16 kg -
Mechanical propertiesValueUnitTest Standard
ISO Data
Yield stress 30 MPa ISO 527-1/-2
Stress at break 17 MPa ISO 527-1/-2
Strain at break >50 % ISO 527-1/-2
Flexural modulus, 23°C 1450 MPa ISO 178
Shore D hardness, 15s 69 - ISO 7619-1
Thermal propertiesValueUnitTest Standard
ISO Data
Melting temperature, 10°C/min 137 °C ISO 11357-1/-3
Other propertiesValueUnitTest Standard
ISO Data
Density 960 kg/m³ ISO 1183
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Features
Low Warpage
Chemical Resistance
Oxidation Resistance
Regional Availability
Europe, Near East/Africa
Disclaimer
Copyright M-Base Engineering+Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from M-Base; this is especially valid for claims of compensation resulting from consequential damages. M-Base explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: 2017-07-26 Source: www.materialdatacenter.com