Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Econamid" in Material Data Center leads to the following information:

Tradename: Econamid
Family: PA6, PA66
Producer: DOMO Chemicals
89 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
ECONAMID FL 6GM3010 PA6-(GF+MD)30
ECONAMID FL 6GB3020 PA6-(GF+GB)30
ECONAMID FL 6G15I1UV1 PA6-GF15
ECONAMID FL 6GM3010H1 PA6-(GF+MD)30
ECONAMID FL 6UV1 PA6
ECONAMID FL 6H1 PA6
ECONAMID FL 6M20 PA6-MD20
ECONAMID FLX 6 PA6
ECONAMID FL 6GB3015 PA6-(GF+GB)30
ECONAMID FL 6H1UV1 PA6
ECONAMID FL 6G15I1H1UV1 PA6-GF15
ECONAMID FR 66I1GTI85A PA66
ECONAMID FL 6 PA6
ECONAMID FNP 6 PA6
ECONAMID FL 6G15 PA6-GF15
ECONAMID FL 6G20 PA6-GF20
ECONAMID FL 6G25 PA6-GF25
ECONAMID FL 6G30 PA6-GF30
ECONAMID FL 6G30 201 PA6-GF30
ECONAMID FL 6G35 PA6-GF35
ECONAMID FL 6G35H1 PA6-GF35
ECONAMID FL 6G35H2 PA6-GF35
ECONAMID FL 6G15 201 PA6-GF15
ECONAMID FL 6G15H1 PA6-GF15
ECONAMID FL 6G20H1 PA6-GF20
ECONAMID FL 6G15UV1 PA6-GF15
ECONAMID FL 6G30H1 PA6-GF30
ECONAMID FL 6G15H1UV1 PA6-GF15
ECONAMID FLX 6G30 PA6-GF30
ECONAMID FL 6G30UV1 PA6-GF30
ECONAMID FL 6G30 500 PA6-GF30
ECONAMID FL 6G15 500 PA6-GF15
ECONAMID PLUS 6G15 PA6-GF15
ECONAMID ORO 6G30 124 PA6-GF30
ECONAMID ORO 6G30 PA6-GF30
ECONAMID ORO 6G15 124 PA6-GF15
ECONAMID FL 6G33 PA6-GF33
ECONAMID FL 6G15H1UV1 500 PA6-GF15
ECONAMID FL 6G15H1 500 PA6-GF15
ECONAMID PLUS 6G30 PA6-GF30
ECONAMID PLUS 6G30 500 PA6-GF30
ECONAMID FL 6B15 PA6-GB15
ECONAMID FL 6B30 PA6-GB30
ECONAMID FL 66B30 PA66-GB30
ECONAMID FL 6M40 PA6-MD40
ECONAMID FL 6M30 PA6-MD30
ECONAMID FL 6M15 PA6-MD15
ECONAMID FL 6M30H1 PA6-MD30
ECONAMID FL 6GM2010 PA6-(GF+MD)20
ECONAMID FL 6M35 PA6-MD35
ECONAMID FL 66M40 PA66-MD40
ECONAMID FL 66 500 PA66
ECONAMID FL 66I1 PA66
ECONAMID FL 66I1H1 PA66
ECONAMID FL 66I2 PA66
ECONAMID FL 66G30 PA66-GF30
ECONAMID FL 66G30UV1 PA66-GF30
ECONAMID FL 66G35H1 PA66-GF35
ECONAMID FL 66/6G35H2 PA666-GF35
ECONAMID FL 66G15 PA66-GF15
ECONAMID FL 66G20 PA66-GF20
ECONAMID FL 66G35 PA66-GF35
ECONAMID FL 66G25 500 PA66-GF25
ECONAMID FL 66G30 503 PA66-GF30
ECONAMID FL 66G25H1 PA66-GF25
ECONAMID FL 66G30H1 PA66-GF30
ECONAMID FL 66G30H1UV1 PA66-GF30
ECONAMID FL 66G25 PA66-GF25
ECONAMID FL 66/6G15 PA666-GF15
ECONAMID FL 66 PA66
ECONAMID FL 66H1 PA66
ECONAMID FL 66/6 PA666
ECONAMID FL 66G40 PA66-GF40
ECONAMID FL 6 500 PA6
ECONAMID FL 6I1 PA6
ECONAMID FL 6I1 401 PA6
ECONAMID FL 6I2 PA6
ECONAMID FR 66G25V0P PA66-GF25
ECONAMID FR 6G30V0E PA6-GF30
ECONAMID FR 6G20V0E PA6-GF20
ECONAMID ORO 6 PA6
ECONAMID PLUS 66G30H1 500 PA66-GF30
ECONAMID PLUS 6G30H2 BK PA6-GF30
ECONAMID FL 6 111 PA6
ECONAMID AIR 66RC10H2 BK99 PA66-CF10
ECONAMID AIR 66RC10H2 NC99 PA66-CF10
ECONAMID AIR 66RC20H2 BK99 PA66-CF20
ECONAMID AIR 66/6RC10H2 BK99 PA666-CF10
ECONAMID AIR 66/6RC10H2 NC99 PA666-CF10

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.