Daiamid - PA - Daicel-Evonik Ltd

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Daiamid" in Material Data Center leads to the following information:

Tradename: Daiamid
Family: PA
Producer: Daicel-Evonik Ltd
35 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
DAIAMID® A1709P PA12
DAIAMID® A6658 PA12-GF
DAIAMID® A6659 PA12-GF35
DAIAMID® A6699 PA12
DAIAMID® A6915 PA12-GF
DAIAMID® E1947 PA12
DAIAMID® E73-K2 PA12
DAIAMID® E75-K2 PA12
DAIAMID® L-GF15 PA12
DAIAMID® L-GF30 PA12
DAIAMID® L1640 PA12
DAIAMID® L1724K PA12
DAIAMID® L1743 PA12
DAIAMID® L1833 PA12
DAIAMID® L1930 PA12
DAIAMID® L1940 PA12
DAIAMID® L1940G30 PA12
DAIAMID® L1940W PA12
DAIAMID® L1960T PA12-Z
DAIAMID® L1965J PA12-P
DAIAMID® L2121 PA12
DAIAMID® L2140 PA12
DAIAMID® L2140W PA12
DAIAMID® X1988 PA12
DAIAMID® X1988W PA12
DAIAMID® X4442 PA12
DAIAMID® X7293 black PA12
DAIAMID® ZE7000 PA12
DAIAMID® ZE7200 PA12-GF
DAIAMID® ZL 1101 PA12
DAIAMID® ZL 1101B PA12
DAIAMID® ZL 1101W PA12
DAIAMID® ZL 1103 PA12
DAIAMID® ZL9501 PA12
DAIAMID® ZZ3000P PA12

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.